EN 10204 3.1 with every batch · Inspection records before loading sales@hongmingmetal.com WhatsApp +86-177-5175-5597 WeChat 17751755597

Grades and reference tables

What Stainless Steel Means: A Film, Not a Grade

Four families sit under one trade name, and the film behind it is thinner than a wavelength of light. What it survives, what breaks it, and why rust still happens.

2026-11-27

Stainless steel is not a steel that cannot stain. It is a steel with enough chromium, 10.5 percent by weight at the minimum, to grow a chromium oxide film on its surface. The film is about 1 to 3 nanometers thick, invisible, and it re-forms within minutes of being scratched, as long as oxygen reaches the metal.

The name is commercial rather than metallurgical. It was coined in Sheffield in the 1910s for a 12 percent chromium cutlery steel, and it survived because it described the benefit instead of the metallurgy. Four different families of steel now sit under that name, and only one of them is what most buyers picture when they read it.

Four families, one word

Austenitic covers the 200 and 300 series: 18/8, 304, 316L, 321. Nickel-stabilized, non-magnetic when annealed, weldable, and the default for anything that has to resist corrosion.

Ferritic covers most of the 400 series: 430, 444. Chromium without nickel, magnetic, cheaper, suited to dry indoor work and trim.

Martensitic is also 400 series: 410, 420, 440C. Hardened by heat treatment and used where wear resistance matters more than corrosion resistance.

Duplex, 2205 and its relatives, is roughly half austenite and half ferrite. High chromium, low nickel, about twice the yield strength of 304 and considerably better under chlorides.

A drawing that says "stainless steel" without a grade could mean any of the four, and they do not substitute for one another.

How the film fails

The film is thin enough that small things matter. Five failure modes account for most of the rust found on stainless parts in service, and each one leaves a different signature.

What you see Failure mode What caused it
Dark pits with a rust bloom on a polished face chloride pitting chloride above what the grade tolerates
Rust lines under a gasket, clamp or lap joint crevice attack stagnant electrolyte, no oxygen renewal
Scattered rust spots after fabrication iron contamination carbon steel particles from a wire brush or shared grinding wheel
Dark oxide along a weld bead, then rust heat tint chromium depleted at the weld, film cannot rebuild
Corrosion beside a weld after months sensitization chromium carbides formed in a standard-carbon grade

The first two are grade and design questions. The last three are fabrication questions, and they are the ones that produce a claim, because the material left the mill in specification.

Stainless, not rustless

304 exposed to coastal air will stain. It is not defective; the environment exceeded what that grade holds. 430 in a dry kitchen is fine and 430 in a dishwasher is not. 316L handles most chloride service and still has a limit, which is why the PREN number exists as a comparison tool.

The practical reading is that "stainless" is a claim about the film, and the film's tolerance is set by the grade and the environment together. A supplier who answers "it is stainless, it will not rust" has answered neither question.

What to write instead

Replace the word with four fields: grade, standard, finish, condition.

  • 316L sheet to ASTM A240, 2B, annealed and pickled
  • 2205 plate to ASTM A240, hot rolled, solution annealed
  • 304 tube to ASTM A312 TP304, 1.5 inch schedule 10

Each of those can be checked against a certificate. "Stainless steel" cannot, and that is the whole difference between a specification and a category.

The film is the product. Everything else on the data sheet describes how well a given steel can keep it.

Have a spec you are not sure about? Send the grade, temper and dimensions — we will tell you what the line can actually hold, and what the certificate will say. Request a quote → Related product range: Stainless Steel Sheet & Plate
Tell us the grade, temper and thickness. Quote within 24 hours.