EN 10204 3.1 with every batch · Inspection records before loading sales@hongmingmetal.com WhatsApp +86-177-5175-5597 WeChat 17751755597

Quality and inspection

Opening the Container: Handling a Stainless Surface Claim

A surface claim is usually lost as soon as the container opens. Photograph the seal and the first bundle in place, separate condensation from contamination and pitting, and send the heat number with the evidence.

2026-11-07

The argument about a stained or scratched stainless surface is usually lost as soon as the container doors open, not in the emails that follow weeks later. Once the bundles are unwrapped, moved into the warehouse and mixed with other stock, there is no photograph that can show where the damage was when it arrived.

Before anything leaves the container

  1. Photograph the seal and the container number before the seal is cut, and keep the seal.
  2. Photograph the first bundle in place, with the shipping mark legible in the frame.
  3. Photograph the packing as it comes apart: wrap, interleaving, desiccants, edge protectors, dunnage.
  4. Keep the packing material from at least one bundle until the claim is closed.

A single close-up of a scratch proves nothing. A dated sequence that shows the mark, the wrap and the position in the container is what lets a supplier and an insurer reconstruct the event.

Separate the four causes before arguing about liability

What you see Usual cause Evidence that settles it
Brown film or water marks across whole faces, often between stacked sheets Condensation during the voyage (container rain) or wet-storage stain Desiccant count and placement, wrap integrity, photos of the sealed stack
Fine parallel scratches on polished or 2B faces Interleaving missing, or grit trapped between faces Photos of the layer stack, protective film condition
Isolated rust spots or streaks along handling lines Free iron from carbon steel tools, slings or racks Distribution pattern, plus a free-iron test on the spot
Pitting on a clean, exposed face Grade under-specified for the service, or heat tint left on a weld Certificate chemistry, service description, weld history

The first three are packing or fabrication problems. The fourth is a material or specification problem. They are settled with different documents, which is why "the whole container is rusty" is not a usable claim.

Evidence a supplier can act on

Send the heat number, the bundle or case number, the contract number, the certificate, the container number and the photographs in one package, with the date the container was opened. The shipping mark should carry the grade and heat or batch number so a crate can be matched to the EN 10204 3.1 certificate without unwrapping another pallet. Where the material has already been cut, add the cutting record.

Ask for packing photographs taken before the container was sealed as well. Those show the condition of the stack at the one moment that cannot be reproduced later. In-process status and photos are available while an order is running, and the quality control page sets out where that record fits.

Clauses that prevent the claim

Clause What to write
Packaging class Wooden case, pallet or bare bundle, named
Surface protection Interleaving between faces, waterproof wrap, protective film where the finish is the product
Moisture control Desiccant quantity per package
Timber Treated to ISPM 15
Marking Product, spec, grade, heat or batch, contract number
Claim evidence Photograph on opening, notify within an agreed window

The export packing specification gives the wording for those lines. Bundle weight limits belong to the buyer, because the receiving yard's lifting gear sets that number, not the mill. For stainless sheet and plate, the surface is often the product, so the packaging class is worth arguing about at quotation rather than after arrival.

Photograph the seal before it is cut and the first bundle before it is lifted. Everything after that is reconstruction.

Have a spec you are not sure about? Send the grade, temper and dimensions — we will tell you what the line can actually hold, and what the certificate will say. Request a quote → Related product range: Stainless Steel Sheet & Plate
Tell us the grade, temper and thickness. Quote within 24 hours.