A276 or A479: What the Bar Was Before It Was Cut

A276 and A479 cover the same shapes and often the same grade. What separates them is what the part has to survive: a code release, a stated condition, and a test direction that follows whatever the bar was before it was cut.

2026-11-25

A276 and A479 both cover stainless bar and shapes. A276 is the general bar standard; A479 is the same shape released for boilers and pressure-retaining parts. The grade number inside the two is usually identical, which is how an order ends up naming one document for a part that needed the other.

Two bar standards, one shape

Plate and pipe sit in their own documents, A240 and A312, so the confusion is rarely about the form. It starts one step later, when the same bar has to be released against a code.

Standard Covers What arrives
A240 / A240M Plate, sheet and strip for pressure vessels and general use Flat, from coil or rolled plate
A276 / A276M Bars and shapes, hot or cold finished Round, square, hex and flat bar
A479 / A479M Bar and shape for boilers and pressure vessels Released against a code

A forged flange sits under A182, and a fitting formed and welded from plate stays A240 material, because welding does not change what the parent product was.

Three differences the grade name hides

The first is test direction. Plate is tension tested across the rolling direction, because that is the weak direction of a rolled product and the direction a formed shell loads. Bar is tested along its length. A yield figure on a plate certificate and the same figure on a bar certificate describe material pulled at right angles to each other, and only one of them is the number your part sees.

The second is condition. A240 requires the austenitic grades to be solution annealed and quenched. A276 allows a bar to be supplied annealed, hot worked, cold drawn, ground or polished, and those conditions do not produce the same mechanicals. Cold-drawn 316L bar is stronger and considerably less ductile than annealed plate of the same grade. If the drawing depends on elongation, "A276 316L" does not buy it. The condition has to be on the order.

The third is acceptance. A bar can satisfy A276 and still fail A479, because A479 adds requirements that only matter once the part holds pressure. A supplier quoting A276 bar against a drawing that names A479 is quoting a different product, however identical the chemistry looks on paper.

The question that settles the substitution

Ask what the material was before it was cut. A ring blanked from 100 mm plate started as plate: the certificate follows the plate. A ring bored from 100 mm round bar started as bar: the certificate is A276 or A479. The finished part is a ring either way. The paperwork is not the same, and neither is the direction the properties were measured in.

The same question decides who carries the traceability. Buy plate and cut it yourself, and the plate certificate is yours while the cut edge is your operation. Buy a cut blank, and the link from that blank back to the parent heat becomes the supplier's obligation, which has to be agreed before the saw starts. Once the offcuts lose their tags, the heat number on the bundle is the only thing that survives.

What belongs in the order

Write this Because
Product standard with the form named: A240 plate, A276 bar, A479 bar Fixes scope before anyone reads the grade
UNS designation beside the common number: S31603, not just 316L Ends the grade-name argument at the dock
Delivery condition: solution annealed, cold drawn, quarter hard A276 does not default to annealed
Certificate type, tied to each heat A 3.1 is not the same document as a 2.2

Two lines do most of the work: the product standard and the condition. The rest is consequence.

The chemistry these documents check does not change with the standard, so the limits for 304 and 316L apply whichever one you name. Where the American and European systems part company on the same grade, A240 against EN 10088 maps it. For an order that carries plate for the shell and bar for the internals, the stainless RFQ guide shows how to keep the two scopes from collapsing into one line.

Have a spec you are not sure about? Send the grade, temper and dimensions — we will tell you what the line can actually hold, and what the certificate will say. Request a quote → Related product range: Stainless Steel Bar & Rod
Tell us the grade, temper and thickness. Quote within 24 hours.
Get a Quote WhatsApp