EN 10204 3.1 with every batch · Inspection records before loading sales@hongmingmetal.com WhatsApp +86-177-5175-5597 WeChat 17751755597

Grades and reference tables

Why a Magnet Does Not Tell You Whether It Is 304

A magnet reads whether steel is ferromagnetic at that spot, not its nickel content. Cold-worked 304 sticks; some 200-series substitutes barely do. Grade acceptance needs the heat number, PMI on nickel and molybdenum, and the certificate chemistry.

2026-11-07

A magnet detects one thing: whether the steel is ferromagnetic at that spot. It cannot read nickel, and nickel is what separates 304 from the 200-series grades offered in its place. A magnet is a sorting tool in a scrapyard, not a grade check at a receiving bay.

Three claims worth dropping

  1. "It sticks, so it is not 304." Annealed austenitic 304 is essentially non-magnetic, but cold work transforms part of the structure to martensite. A sheared edge, a bent tube or a deeply drawn sink can hold a magnet while the chemistry is still squarely 304. Solution annealing restores the non-magnetic condition.

  2. "It does not stick, so it is 304." Ferritic 430 is magnetic, some 200-series material is weakly so or nearly not, and a fully annealed austenitic sheet gives the same result as a correctly labeled one. Absence of attraction proves nothing about nickel.

  3. "A spark test or an acid drop kit settles it." Both are screens. They separate families of steel, and neither produces the composition line by line that a purchase order is written against.

What the certificate and a PMI gun can tell you

ASTM A240 gives 304 as chromium 18.0 to 20.0 and nickel 8.0 to 10.5, with carbon at 0.08 max. A 200-series substitute replaces part of that nickel with manganese, so the number to look at is nickel, not whether the sheet is magnetic. 316L is separated from 304 by molybdenum, 2.00 to 3.00 under the same standard, which is exactly the element a handheld XRF reads well.

What XRF does not read is carbon. The L grades carry a carbon limit of 0.030 max under ASTM A240, and that value has to come from the heat analysis on the certificate. The two checks are complementary: PMI catches a substitution in front of you, the certificate carries the carbon and nitrogen that PMI cannot.

A workable sequence at the receiving bay

  • Match the heat number on the bundle mark to the 3.1 certificate before anyone cuts into the pack.
  • Run PMI on the pieces that matter and record nickel and molybdenum, not just the grade name the gun prints.
  • Read the chemistry on the certificate against the ordered standard, including carbon, before releasing the lot.

The 304 grade page keeps the composition limits and the standard references together. A magnet is useful for separating mixed stock in the yard. It has no place in the acceptance decision.

Have a spec you are not sure about? Send the grade, temper and dimensions — we will tell you what the line can actually hold, and what the certificate will say. Request a quote → Related product range: Stainless Steel Sheet & Plate
Tell us the grade, temper and thickness. Quote within 24 hours.
Get a Quote WhatsApp